MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

General Plastics LAST-A-FOAM® FR-4718 Foam
Categories: Other Engineering Material

Material Notes: Product Description: The FR-4700 is a rigid, high-temperature, hybrid tooling board that is non-abrasive and can be machined and cut with HSS cutters or any standard cutting tool. It can be bonded to itself or other substrates using urethane or epoxy adhesives.

Key Performance Benefits:

  • Applications up to 400°F peak temperature
  • High-temperature continuous use up to 350°F
  • Compatible with commercial pre-pregs
  • No outgassing or cure inhibition
  • Dimensionally stable
  • Large block sizes available
  • Reduced bond lines
  • Reduced bonding labor
  • Excellent surface finish
  • Easy machinability
Applications:
  • Prototype machining
  • Prepreg composite layup tooling
  • Vacuum form tooling
  • Tool proofing
  • Pattern making
  • Master model making

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.288 g/cc0.0104 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.00 MPa290 psiASTM D1623
Flexural Strength 1.94 MPa282 psiASTM D790
Flexural Modulus 0.0979 GPa14.2 ksiASTM D790
Compressive Strength  2.67 MPa
@Temperature 177 °C
387 psi
@Temperature 350 °F
Perpendicular to Rise; ASTM D1621
 4.59 MPa
@Temperature 177 °C
665 psi
@Temperature 350 °F
Parallel to Rise; ASTM D1621
 7.336 MPa
@Temperature 23.9 °C
1064 psi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
 9.294 MPa
@Temperature 23.9 °C
1348 psi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
Compressive Modulus  0.069237 GPa
@Temperature 177 °C
10.042 ksi
@Temperature 350 °F
Perpendicular to Rise; ASTM D1621
 0.18010 GPa
@Temperature 177 °C
26.121 ksi
@Temperature 350 °F
Parallel to Rise; ASTM D1621
 0.21902 GPa
@Temperature 23.9 °C
31.766 ksi
@Temperature 75.0 °F
Perpendicular to Rise; ASTM D1621
 0.32016 GPa
@Temperature 23.9 °C
46.435 ksi
@Temperature 75.0 °F
Parallel to Rise; ASTM D1621
 
Thermal PropertiesMetricEnglishComments
CTE, linear  45.0 µm/m-°C
@Temperature 23.9 - 204 °C
25.0 µin/in-°F
@Temperature 75.0 - 400 °F
ASTM E831
 48.6 µm/m-°C
@Temperature -45.6 - 93.3 °C
27.0 µin/in-°F
@Temperature -50.0 - 200 °F
GP Method
Thermal Conductivity 0.0605 W/m-K0.420 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 177 °C350 °F
Glass Transition Temp, Tg 220 °C428 °FASTM E1545

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay LTF 318B
Solvay CYFORM® 22 Epoxy Tooling Prepreg
Lord Adhesives Circalok™ EP-729 Epoxy Board Level Encapsulant
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
Hexcel® F161 Epoxy Resin

PGENR034 / 186820

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.