MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYBLAK™ 2076 Superior Black Color Concentrate, 40% Carbon Black Based In EVA
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Description

POLYBLAK® Black 2076 is a superior black color concentrate containing 40% carbon black in EVA. This masterbatch is designed to provide good opacity and a regular blue undertone with pigment particle size of 70 nanometers. POLYBLAK® Black 2076 is formulated for use in injection molding applications. POLYBLAK® Black 2076 is typically recommended for use at 5% addition levels.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Moisture Absorption <= 0.100 %ASTM D789
Carbon Black Loading 40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Evatane® 1003 VL 2 Ethylene Vinyl Acetate
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Arkema Orevac® 9305 Film EVA-MAH Terpolymer
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam
Celanese Ateva® 1608 EVA polymer for compounds, molding and tubing

PASHU526 / 25490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.