MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell ACCUGLASS® PTTY P-112LS Spin-on Glass
Categories: Ceramic; Glass

Material Notes: The ACCUGLASS P-TTY Spin-on Glass (SOG) Series (κ = 4.1-4.3) is a family of phosphosilicate polymers used for metal and poly planarization, overcoat passivation and non-etchback interlayer dielectric in the manufacture of integrated circuits. The ACCUGLASS P-TTY series also provides Na+ gettering ability similar to P-doped CVD oxides. The ACCUGLASS P-TTY series contains 2wt% (P-112A), 2.7wt% (P-112LS) and 4wt% (P-114A) phosphorous bonded to O atoms in the Si-O backbone. The spec-ific formulation results in a stable dielectric constant, <2% within wafer uniformity and can be densified at temperatures up to 700-900°C with no significant loss of phosphorous. Thin films of ACCUGLASS P-TTY are applied using a commercial coater and cured in a vertical or horizontal furnace to thicknesses up to 1000Å (single coat) and 2000Å (double coat). Typically, two coats at ~1,000Å each are applied with hot plate bakes in between coats to achieve optimum planarization.

Benefits

  • Industry proven performance and broad acceptance in subtractive aluminum processing
  • Phosphorus stability up to 900°C
  • Thickness variation within a wafer of less than 2%
  • P-112Ls has similar etch properties as BPSG
Applications:
  • PMD-BPSG Planarization
  • Overcoat Passivation
  • ILD Planarization
  • Available in both Etchback and Non-Etchback
Accuglass P-TTY is suitable for metal and poly planarization, partial and non-etchback applications in a CVD/SOG/CVD sandwich structure. ACCUGLASS P-TTY can also be used for overcoat passivation.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 100 MPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.1
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 µm/m-°C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.44
@Wavelength 633 nm
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 4.00 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell ACCUGLASS® P-5S Spin-on Glass
Honeywell ACCUGLASS® T11 311 Spin-on Glass
Honeywell ACCUGLASS® T11 111 Spin-on Glass
Honeywell ACCUGLASS® PTTY P-114A Spin-on Glass
Honeywell ACCUGLASS® PTTY P-112A Spin-on Glass

PHONWL074 / 179619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.