MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Avient Synprene® RT-5190 Thermoplastic Elastomer - SBC  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:

Description/Features:

  • High Performance Thermoplastic Elastomer
  • Natural
  • Ignition Resistant

Applications:

  • Multi-Purpose

Market:

  • Building and Construction
  • Consumer Goods
  • Industrial

Processing Method:

  • Injection Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 333310 Sec; ASTM D2240
Tensile Strength at Break 13.8 MPa2000 psiMethod A (Dumbbell & Section), 20 in/min; ASTM D412
Tensile Stress at Strain 7.93 MPa
@Strain 300 %
1150 psi
@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 625 %625 %Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 37 %37 %Bayshore; ASTM D2632
Tear Strength 57.8 kN/m330 pliDie C (graves), 20 in/min; ASTM D624
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -50.0 °C-58.0 °FASTM D746
Flammability, UL94 V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0620 in
Natural; UL 94
Oxygen Index 27 %27 %0.062 in. bars; ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PO3320 / 45007

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.