MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ganpati Exim N - 550 Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Medium reinforcing carbon black with medium dispersion. Provides high extrusion ability, comparatively high tear resistance. Tire body and tube compounds. Profile-extruded products. Industrial rubber goods, seals, hoses.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.335 - 0.395 g/ccPour
pH 6.0 - 8.0
Specific Surface Area 39 m²/gExternal; Statistical Thickness Surface Area,; ASTM D 6556
 37 - 47 m²/gExternal
Ash <= 0.45 %
 
Mechanical PropertiesOriginal ValueComments
300% Modulus 0.700 - 2.70 MPaIRB 6
 
Descriptive Properties
Carbon Black Temperature in a Hopper Car<65°C
Content<0.15%Toluene Extractables
 <1.1%Sulphur
DBP Absorption Number117-125 cm3/100g
DBP Absorption Number of Compressed Sample83-93 cm3/100g
Fines Content<7%Pelleted
Heating Loss<0.9%
Individual Pellet Hardness25-100 g
Iodine Number38-48 g/kg
Nitrogen Adsorption Number40 m2/g(D6556)
Sieve Residue<0.001%05
 <0.1%0045
Toluene Discoloration>90%transmittance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI008 / 317292

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.