MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NOVA Chemicals NOVAPOL® PF-Y818-FX LLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Butene Copolymer

Features:

  • Moderate toughness
  • Superior melt-strength for high output film lines
  • Blends well with LDPE

Additives:

  • Base resin
  • Process stabilizer

Applications:

  • Food packaging
  • Industrial packaging
  • Liners

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 100-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL PF-Y818-FX resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D 792
Thickness 25.0 microns
Melt Index of Compound 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPaASTM D 882
Film Tensile Strength at Yield, TD 11.0 MPaASTM D 882
Film Elongation at Break, MD 500 %ASTM D 882
Film Elongation at Break, TD 810 %ASTM D 882
Elmendorf Tear Strength MD 50 gASTM D 1922
Elmendorf Tear Strength TD 475 gASTM D 1922
Dart Drop Test 115 gF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 47.0 MPaASTM D 882
Film Tensile Strength at Break, TD 33.0 MPaASTM D 882
1% Secant Modulus, MD 175 MPaASTM D 882
1% Secant Modulus, TD 230 MPaASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM D 1003
Gloss 65 %@ 45°; ASTM D 2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)84NOVA Chemicals Test Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 25 Micron Film
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin

PNOVB008 / 194616

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.