MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem® Emulsion 91240G Nonionic polyethylene emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Nonionic polyethylene emulsion

Usage: Michem® Emulsion 91240G is an additive which provides excellent anti-blocking, slip properties and mar resistance. It is also used as an additive for inks, coatings and OPV where it imparts gloss and scratch resistance.

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 - 1.01 g/cc0.990 - 1.01 g/cc
Volatiles 59.5 - 60.5 %59.5 - 60.5 %
pH 5.0 - 8.05.0 - 8.0
 2.0 - 122.0 - 12Recommended pH of system
Brookfield Viscosity <= 300 cP<= 300 cPSpindle # 2, rpm 60
 
Descriptive Properties
AppearanceWhite liquid
Emulsifier ChargeNonionic
Solids TypePolyethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP30DPMed USP Class VI, Two Component Epoxy Urethane System
Northstar Polymers MSS-A85C Ester Base Polyurethane
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane
DSM Biomedical Bionate® 80A Thermoplastic Polycarbonate Polyurethane (PCU)

WMICHEL107 / 135024

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.