MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT ALPA-SIL CLEAR Silicone Molding Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: This is a pourable 2-part addition cure silicone elastomer system. After mixing parts ‘A’ and ‘B’ in the correct proportions, the system will cure at ambient temperatures within 24 hours, but the rate of cure can be accelerated by heat. The cured rubber exhibits excellent physical and electrical properties.

Key Features

  • Crosslinks at temperatures as of 23 °C/77°F
  • High flowing capacity
  • Easy mixing of the components
  • Excellent reproduction fidelity of details
Application: For dental laboratories and for producing otoplastics.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³A; BS ISO 2781
 0.980 g/cc0.0354 lb/in³B; BS ISO 2781
Brookfield Viscosity 7500 cP7500 cPA
 7500 cP7500 cPB
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2020DIN 53 505
Elongation at Break 200 %200 %ISO 37
Tear Strength 2.98 kN/m17.0 pliBS ISO 34-1
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min0.500 hourDe-mould Time / Full Cure
Pot Life 2.50 min2.50 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColortransparentA
 transparentCured Product
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL104 / 314587

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.