MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terluran® HI-10 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Terluran® HI-10 is an medium flow, injection molding grade with very high resistance to impact with excellent heat distortion and suitable for injection molding and extrusion. High toughness, Very high impact, Medium flow, Great mechanical strength and rigidity, High impact at sub-zero temperatures.

Applications: Injection molding, Compounding, Appliance housings, Lawn & garden components requiring superior toughness

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Moisture Absorption at Equilibrium 0.21 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 1.03 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 5.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM Test
Ball Indentation Hardness 74.0 MPaISO 2039-1
Tensile Strength, Yield 38.0 MPaISO 527
Elongation at Break 9.0 %Nominal; ISO 527
Elongation at Yield 2.8 %ISO 527
Tensile Modulus 1900 MPaISO 527
Flexural Strength 56.0 MPaISO 178
Izod Impact, Notched 120 J/m
@Temperature -30.0 °C
ASTM Test
 180 J/m
@Temperature -18.0 °C
ASTM Test
 4.50 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 14.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 36.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 140 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 35.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0054
@Frequency 100 Hz
IEC 60250
 0.0082
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 110 µm/m-°CISO 11359
Thermal Conductivity 0.170 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 90.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 103 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Yellow Index 15 %DIN 6167
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 260 °CISO 294
Mold Temperature 30.0 - 80.0 °CISO 294
Injection Velocity 200 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
 
Compliance PropertiesOriginal ValueComments
FDA Yes
NSF NoNSF Std. 61
 YesNSF Std. 51
USP Class VI No
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® HI-12 ABS
Chi Mei Polylac® PA-757 ABS
INEOS Styrolution Terluran® GP-22 ABS
LG Chemical HI-121 ABS, High Impact
LG Chemical HI100 ABS, High Impact

PBASF9053 / 84817

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.