MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Syncure™ System S107FH Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: UL Bullentinized, silane-grafted (2-step) moisture crosslinkable polyethylene system, UL 90°C.

Typical Properties measured on 18 AWG with 30 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.948 g/ccASTM D792
Deformation 10 %
@Temperature 131 °C
UL 1581
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5910 sec; ASTM D2240
 64ASTM D2240
Tensile Strength, Yield 31.0 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 400 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.5
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °CUL Temperature Rating
 
Descriptive Properties
Agency RatingsCSA, C-22.2, No. 127, Type CL-1251
 UL 758
Catalyst Masterbatch33%V-0045G RoHS
FormsPellets
Gel Content72%ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Grafted Base Resin67%S-1054A
Processing MethodExtrusion Coating
Regional AvailabilityNorth America
Retention of Tensile Elongation75%158°C, 1.91 mm; 672 hr, UL Standard
Retention of Tensile Strength75%158°C, 1.91 mm; 672 hr, UL Standard
UsesAppliances
 Wire & Cable Applications
Wire TypesAWM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis Borlink™ LE4244S Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE0592S Polyethylene
Avient Syncure™ V0064G Crosslinked Polyethylene (XLPE)
Avient Syncure™ V0044G S-1 RoHS Natural Polyethylene, Crosslinked (XLPE)

PH0POL0322 / 144891

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.