MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Resin Technology Group UV-406 High Clarity, Moisture Resistant, UV Curing Bonder
Categories: Polymer; Adhesive; Thermoset

Material Notes: UV 406 is a rapidly curing UV adhesive developed for use in bonding a variety of plastics, glass and metals, where moisture resistance and low shrinkage during cure is critical. Bond strengths on polycarbonate and rigid and flexible PVC usually exceed the strength of those substrates. UV 406 has excellent wetting capabilities. Bond lines are clear and colorless.

Applications:

Decal plates, Fiberoptic bonding, Globtop coating, Glass assembly, Head lamps, Micro-Electronic encapsulation.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccUncured
Water Absorption 1.0 %Cured
Viscosity 60 - 100 cP
@Temperature 25.0 °C
Uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85Cured
Tensile Strength at Break 6000 psiCured
Elongation at Break 12 %Cured
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 750 V/milCured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °CCured
Minimum Service Temperature, Air -54.0 °CCured
Flash Point >= 200 °FUncured
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. Specifies clear but does not quantify
 
Descriptive Properties
ColorClear
CompositionUrethane Oligomer/ (Meth) Acrylate Monomer Blend
SolubilityAlcohol, Chlorinated solvents
ToxicityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESINT642 / 65526

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.