Description: BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, oil and solvent resistance and creep resistance at elevated temperatures. Typical applications include replacements for die castings and sheet molding compounds, cylinder head covers, engine front timing covers, oil pans and structural components.Information provided by Bulk Molding Compounds |