MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.

Films manufactured with Eraclene FA 706 show good processability together with high temperature resistance and good tensile properties at low strain (Young modulus, yield strength).

Main Applications: Eraclene FA 706 is especially recommended for the production of "paper-like" films having high stiffness together with high thermal resistance. Due to its excellent compromise between drawability and bubble stability, Eraclene FA 706 is the ideal choice for manufacturing of high strength thin films (shopping bags, bags on the reel, lamination films).

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.952 g/ccISO 1183
Thickness 10.0 - 50.0 micronsRecommended
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 8.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %ISO 527-3
Film Elongation at Break, TD 450 %ISO 527-3
Elmendorf Tear Strength, MD 1.019 g/micronISO 6383-2
Elmendorf Tear Strength, TD 2.5475 g/micronISO 6383-2
Dart Drop Test 100 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 46.0 MPaISO 527-3
Film Tensile Strength at Break, TD 48.0 MPaISO 527-3
1% Secant Modulus, MD 760 MPaISO 527-3
1% Secant Modulus, TD 830 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 134 °CInternal method
Vicat Softening Point 127 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -60.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Versalis Clearflex® CL 508 Octene Copolymer Linear Medium Density Polyethylene
Versalis Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene

PENG130 / 124524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.