System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical LUPOX GP1000KM PBT, Injection Molding
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Unreinforced, Molded
Material Notes:
High Flow, High Impact
Application: Automotive (Connector)
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.28
g/cc
0.0462
lb/in³
ASTM D792
Water Absorption
0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage
0.012
-
0.020
cm/cm
0.012
-
0.020
in/in
ASTM D955
Melt Flow
54
g/10 min
@Load 2.16 kg,
Temperature 250 °C
54
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
45.1
MPa
@Thickness 3.20 mm
6540
psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break
100 %
@Thickness 3.20 mm
100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Strength
68.6
MPa
@Thickness 3.20 mm
9950
psi
@Thickness 0.126 in
2.5mm/min; ASTM D790
Flexural Modulus
1.91
GPa
@Thickness 3.20 mm
277
ksi
@Thickness 0.126 in
2.5mm/min; ASTM D790
Izod Impact, Notched
0.588
J/cm
@Thickness 6.40 mm
1.10
ft-lb/in
@Thickness 0.252 in
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+17
ohm-cm
1.00e+17
ohm-cm
ASTM D 257
Dielectric Strength
23.0
kV/mm
@Thickness 1.00 mm
584
kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance
120
-
179
sec
120
-
179
sec
ASTM D495
Comparative Tracking Index
>=
600
V
>=
600
V
Solution A; UL 746
Thermal Properties
Metric
English
Comments
Melting Point
223
°C
433
°F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi)
58.0
°C
@Thickness 6.40 mm
136
°F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical
140
°C
284
°F
UL 746B
UL RTI, Mechanical with Impact
130
°C
266
°F
UL 746B
UL RTI, Mechanical without Impact
140
°C
284
°F
UL 746B
Flammability, UL94
HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
HB
@Thickness 3.30 mm
HB
@Thickness 0.130 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
230
-
235
°C
446
-
455
°F
Middle Barrel Temperature
235
-
240
°C
455
-
464
°F
Front Barrel Temperature
240
-
245
°C
464
-
473
°F
Nozzle Temperature
240
-
250
°C
464
-
482
°F
Melt Temperature
240
-
250
°C
464
-
482
°F
Mold Temperature
40.0
-
80.0
°C
104
-
176
°F
Drying Temperature
100
-
120
°C
@Time 14400 - 21600 sec
212
-
248
°F
@Time 4.00 - 6.00 hour
Moisture Content
<= 0.020 %
<= 0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLHCHEM9736 / 239260
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.