MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 216 V40 PA6, 40% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.

Benefits: The product offers a good combination between thermal and mechanical properties.

Available in: Europe and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183/A
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 215 MPaISO 527 Type 1A
Elongation at Break 2.3 %ISO 527 Type 1A
Tensile Modulus 13100 MPaISO 527 Type 1A
Flexural Modulus 13000 MPaISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 107 kJ/m²ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 550 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357
Crystallization Temperature 190 °CISO 11357
Flammability, UL94 HB
@Thickness 0.400 mm
1210
 HB
@Thickness 0.800 mm
1210
 HB
@Thickness 1.60 mm
1210
 HB
@Thickness 3.20 mm
1210
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 225 - 230 °C
Front Barrel Temperature 240 - 250 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone230-240°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY
Domo TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY
Domo Technyl® A 216 V40 40% Glass Filled Nylon 66
Domo TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned
Domo TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned

PRHOD759 / 137990

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.