MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta RM320H Rolled and Molded Rod, Cotton Fabric with Phenolic Resin System
Categories: Polymer; Thermoset; Phenolic

Material Notes: Being a heat treated version of RM320, RM320H Rolled and Molded Rods are made from a fine weave (linen) cotton fabric combined with a phenolic resin system. RM320H is used for electrical and mechanical applications.

Information provided by Norplex Micarta.

Key Words: Cotton Fiber, Phenolic
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 95.095.0
Tensile Strength 75.8 MPa11000 psiCondition A
Flexural Strength 138 MPa20000 psiCondition A
Compressive Strength 200 MPa29000 psiCondition A
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 135 °C275 °F
UL RTI, Mechanical with Impact 135 °C275 °F
Flammability, UL94 HBHBCondition A
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.800 %0.800 %Condition D; ASTM D-349
 
Descriptive Properties
Rod Diameter0.5 inch (1.3 mm)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNORPM906 / 323343

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.