3M™ Gripping Material GM400 is based on 3M’s proprietary micro-replicated technology. 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM 110 consists of a high-friction surface with a nylon knit backing that provides stretch in the cross-web direction. It can be attached to other substrates by sewing. 3M gripping material GM110 is ideally suited for applications requiring stretch, such as athletic gloves. When used alone on a single surface 3M gripping material provides a strong secure grip. Then used as a two-part system, for example on a glove and a handlebar grip, strength is maximized. As firmly as 3M gripping material holds, it releases just as easilyInformation provided by 3M |