MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ MEGARAD 2080-10 Polycarbonate, Gamma Radiation Resistant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: CALIBRE™ MEGARAD 2081-10 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (gamma or electronic beam). CALIBRE™ MEGARAD 2081-10 resin can reduce the color shift by 50% compared to general purpose polycarbonate resins. CALIBRE™ 2081-10 resin has undergone biocompatibility testing base on ISO 10993 (biological Evaluation of Medical Devices) and is suitable for use in approved medical applications.

Main Characteristics:

  • Stabilized for high energy radiation
  • Tested under ISO 10993
  • Contains mold release
Application:
  • Medical applications

Data provided by Dow Chemical.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.32 %Equilibrium; ASTM D570
 0.15 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmFlow; ASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 68.0 MPaISO 527-2/50
Tensile Strength, Yield 62.0 MPaISO 527-2/50
Elongation at Break 150 %ISO 527-2/50
Elongation at Yield 6.0 %ISO 527-2/50
Tensile Modulus 2.21 GPaISO 527-2/50
Izod Impact, Notched 750 J/cmASTM D256
Izod Impact, Notched (ISO) 78.0 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) NBISO 180
Charpy Impact, Notched 3.50 J/cm²ISO 179/1eA
Tensile Impact Strength 378 kJ/m²ASTM D1822
Instrumented Impact Total Energy 81.3 J
@Temperature 23.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.00010
@Frequency 60 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 140 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °CUnannealed; ISO 75-2/A
 122 °CUnannealed; ASTM D648
 137 °CAnnealed; ASTM D648
Vicat Softening Point 143 °CISO 306/B50
 148 °CRate A (50°C/h), Loading 2 (50N); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 1.1 %
Transmission, Visible 89 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ MEGARAD™ 2081-15 Polycarbonate Resin
Trinseo CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant
Covestro Makrolon® DP 1-1413 Polycarbonate, Gamma Radiation Stabilized
Schott RS 253 Radiation Shielding Glass
Trinseo CALIBRE™ 5101-8 Polycarbonate Resin

PZZDW039 / 34270

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.