MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Zelux® Polycarbonate 10% Glass Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: Zelux® M GF is a machine grade glass reinforced polycarbonate (PC) with glass loadings from 10% to 40%. These products offer excellent dimensional stability, and greater strength and stiffness at both room and elevated temperatures when compared to unfilled polycarbonate. These products have good insulating properties.

Colors Available: Black; Natural

Attributes: Heat Resistant; Dimensional Stability; Stiffness

Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccASTM D792
Water Absorption 0.12 %ASTM D570; 24 hrs.
Water Absorption at Saturation 0.31 %ASTM D570; at equilibrium
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D7852
Hardness, Rockwell R 124ASTM D7852
Tensile Strength at Break 8000 psiASTM D638
Tensile Strength, Yield 9600 psiASTM D638
Elongation at Break 15 %ASTM D638
Elongation at Yield 8.0 %ASTM D638
Tensile Modulus 450000 psiASTM D638
Flexural Yield Strength 15000 psiASTM D790
Flexural Modulus 500000 psiASTM D790
Compressive Strength 14000 psiASTM D695
Compressive Modulus 520000 psiASTM D695
Izod Impact, Notched 2.00 ft-lb/inASTM D256
Izod Impact, Unnotched 40.0 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 60 Hz
ASTM D150
Dielectric Strength 45.0 kV/mmASTM D149
Dissipation Factor 0.00080
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 1.39 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 295 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 288 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.47 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Zelux® 20% GF Polycarbonate
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber
Westlake Plastics Zelux® 30% GF Polycarbonate
Westlake Plastics Zelux® 40% GF Polycarbonate

PWEST012 / 72716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.