MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Flexible R3090S Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6615 sec; ASTM D2240
Tensile Strength, Yield 11.0 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 370 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -34.0 °CASTM D746
Flammability, UL94 V-2
@Thickness 1.50 mm
BK; Internal Method
 V-2
@Thickness 1.50 mm
NC; Internal Method
 V-2
@Thickness 1.50 mm
RD; Internal Method
Oxygen Index 21 %
@Thickness 1.91 mm
ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 155 - 165 °C
 
Component Elements PropertiesOriginal ValueComments
Sulfate, SO4 <= 0.0050 %
 
Descriptive Properties
Agency RatingsUL QMFZ2
AppearanceClear/Transparent
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Tensile Elongation80%136°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength110%136°C, 1.91 mm; 168 hr, UL Standard
RoHS ComplianceRoHS Compliant
UsesCable Jacketing
 Flexible Cord Jacketing
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible
Sylvin Technologies 9812A-70 Natural PVC for Injection Molding
Fainplast Compounds PH 66/A Flexible PVC, Transparent Extrusion
AlphaGary PVC GM 5065 Natural Polyvinyl Chloride Thermoplastic

PH0POL0311 / 144880

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.