MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Geon® Performance Solutions Vinyl Wire & Cable 3311-xx23D Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 767615 sec; ASTM D2240
Tensile Strength, Yield 53.1 MPa7700 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 150 %150 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 75.0 °C167 °FUL Temperature Rating
Flammability, UL94 V-0
@Thickness 0.749 mm
V-0
@Thickness 0.0295 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
AdditiveLead Stabilizer
Agency RatingsUL QMFZ2
AppearanceClear/Transparent
FeaturesFlame Retardant
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Zelux® CN-P Polycarbonate (conductive)
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative)
Overview of materials for PVC, Extruded
Geon® Performance Solutions Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Rigid Extrusion LR840 Polyvinyl Chloride, Rigid

PH0POL0376 / 144945

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.