MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® C 218 V30 BLACK 21N Nylon 6, 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Product Description: Ultramid® C 218 V30 BLACK 21N is a polyamid 6, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product offers an excellent combination between thermal and mechanical properties.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer

Features: Good Dimensional Stability; Good Flow; Good Mold Release; Heat Stabilized - Inorganic

Uses: Automotive Applications; Connectors; Electrical/Electronic Applications

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527-2
Elongation at Break 6.5 %6.5 %ISO 527-2
Tensile Modulus 6.00 GPa870 ksiISO 527-1
Flexural Strength 160 MPa23200 psiISO 178
Flexural Modulus 5.10 GPa740 ksiISO 178
Izod Impact, Notched (ISO) 18.9 kJ/m²9.00 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 9.03 J/cm²43.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.81 J/cm²8.60 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 62631-3-2
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
560 kV/in
@Thickness 0.0787 in
IEC 60243-1
Comparative Tracking Index 400 V400 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 235 °C446 - 455 °F
Middle Barrel Temperature 235 - 240 °C455 - 464 °F
Front Barrel Temperature 240 - 250 °C464 - 482 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2060 / 310753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.