MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elix Polymers Elix™ M220 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: General purpose grade for self coloring. Main Applications: Household appliances, Housings (phone, computer, printer). Automotive interior, Automotive exterior, Toys, Cosmetics packaging, Extruded sheets, Medical devices, Electroplating, Pipes, Covers, Smart cards.

Property data measured at 23°C and 50% RH.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 3.00 mm
150x105 mm; acc. ISO 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Thickness 3.00 mm
150x105 mm; acc. ISO 2577
Melt Flow 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min MVR; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 103 MPaISO 2039-1
Tensile Strength, Yield 41.0 MPa50 mm/min; ISO 527-1,2
Tensile Modulus 2300 MPa1mm/min.; ISO 527-1,2
Flexural Strength 65.0 MPa2mm/min; ISO 178
Flexural Modulus 2200 MPa2mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 100 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 100 Hz
IEC 60250
 2.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.0073
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,2
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CISO 75-1,2
Vicat Softening Point 95.0 °C50N 50°C/h; ISO 306
 97.0 °C50N 50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °Cinjection molding; ISO 294
Mold Temperature 80.0 °Cinjection molding; ISO 294
Injection Velocity 240 mm/secinjection molding; ISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers ELIX ABS P2H-AT Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Terluran® GP-35 ABS
Lotte Advanced Materials Starex® HG-0760 ABS, Unreinforced
Elix Polymers Elix™ P2H-AT ABS Polymer
Sax Polymers SAXLAC 835U Acrylonitrile Butadiene Styrene

PELIX903 / 192498

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.