MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® QF-180™ Coating Cement
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Fiberfrax QF-180™, QF-180™ Blue, and QF-150™ coating cements provide a range of consistencies for brush, spray, and trowel-on application. These coatings have 1260°C (2300°F) temperature grade rating. They posses good adhesion, thermal reflectance, dielectric strength, hot gas erosion resistance, and effectively resist wetting by many nonferrous molten metals.

    Typical Applications
  • Electrical insulation coatings and potting
  • Adhesive for other Fiberfrax product forms
  • Surface coating for other Fiberfrax product forms
  • Radiant coatings for variety of substances
  • Flame-resistant coatings
  • Surface coating for molten aluminum contact
  • Oxidation-resistant coating for injection tubes and graphite crucibles

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.74 g/cc0.0628 lb/in³
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 1.54 kV/mm39.0 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C30.0 µin/in-°F
Maximum Service Temperature, Air 1177 °C2151 °FRecommended Operating Temperature
Shrinkage 3.2 %
@Temperature 1260 °C,
Time 86400 sec
3.2 %
@Temperature 2300 °F,
Time 24.0 hour
Linear
 
Component Elements PropertiesMetricEnglishComments
Al2O3 37.2 %37.2 %
Fe2O3 0.70 %0.70 %
MgO 0.30 %0.30 %
NaO2 0.70 %0.70 %
SiO2 59.1 %59.1 %
TiO2 1.4 %1.4 %
 
Descriptive Properties
AppearanceWhite paint
Approx. Coverage 1-Layer (SF/Gal)50-100
Temperature Grade (°F)2300
Trace Inorganics (%)0.6
U.S. Coast Guard for "Incombustible Materials" Subpart 164.009X

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CUNIF038 / 97810

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.