Product Description: QGel 323Y is a soft, tough, moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection. Key Features: - One to one mix ratio
- 30 minute cure time at 150°C
- Dispensing equipment recommended
Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |