MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayfol® UV-1 7-2 000000 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Bayfol UV 1 7-2 000000 is an enhanced extrusion lamination film based on Makrolon® polycarbonate.

Properties / Applications: Bayfol UV 1 7-2 000000 is virtually glare-free and has excellent scratch resistance, has been developed especially for critical graphic applications to provide UV resistance. Typical applications are gas pump graphics, harsh exterior environments, nameplates and labels. Bayfol UV 1 7-2 000000 is available in various standard thicknesses from 0.007" to 0.030" (175 microns to 750 microns). Other thicknesses are available on request. The surface combination of Bayfol UV 1 7-2 000000 is one side velvet and one side very fine matte. As with any product, use of Bayfol UV 1 7-2 000000 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Water Absorption 0.40 %
@Time 86400 sec
immersion; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 51.0 MPaASTM D882
Tensile Strength, Yield 51.7 MPaASTM D882
Elongation at Break 110 %ASTM D882
Tear Strength 1110 pliInitiation; ASTM D1004
 
Optical PropertiesOriginal ValueComments
Haze >= 0.90 %ASTM D1003
Gloss 4.0 - 9.0 %60° top side; ASTM D2457
Yellow Index 1.0 %ASTM E313
Transmission, Visible >= 70 %
@Thickness >=0.508 mm
ASTM D1003
 >= 80 %
@Thickness <=0.508 mm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite Hygard® BR1000 Polycarbonate Laminate
Covestro Makroblend® UT6007 PC+PBT
Covestro Makroblend® UT3907 PC+PBT
Covestro Makrolon® OP-V sheet Polycarbonate
Covestro Makrolon® 2/8-10.5 Multi UV sheet, 8 mm Polycarbonate

PCOVEST0142 / 201925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.