MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Huafon T25 Textile Yarn Resin
Categories: Other Engineering Material

Material Notes: Product Description: T25 is light low viscosity.

Typical Applications: T25 can be widely used in nylon 66 staple textile, well applied for auto safe gasbag fiber after solid state post-condensation.

Information provided by Zhejiang Haufon New Materials Corp., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Viscosity 2.48 - 2.56 cP2.48 - 2.56 cPWet Chips
 2.52 - 2.6 cP2.52 - 2.6 cPDry Chips
 
Thermal PropertiesMetricEnglishComments
Melting Point 260.2 °C500.4 °F10°C/min; ASTM D3418
 
Descriptive Properties
NH256-54 mmol/kgDry Chips
 57-55 mmol/kgWet Chips
Particle size1.7-2.3 g/100 Pellets
Water content<5000 mg/kgWet Chips
 <800 mg/kgDry Chips

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUAF285 / 295228

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.