MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem HP FeSi 75 0.05 Ti High Purity Ferrosilicon
Categories: Metal

Material Notes: Apart from being a powerful deoxidizer - because of its strong affinity for oxygen - silicon has an important influence on the properties of steel, depending on the amount used and the combined effect with other elements. Silicon increases namely strength and wear resistance, elasticity (spring steels), scale resistance (heat resistant steels), and lowers electrical conductivity and magnetostriction (electrical steels).

HP FeSi is used when stringent demands are put on steel cleanliness. Compared to regular ferrosilicon, HP FeSi will help to keep both the content of inclusions and the carbon content in the final steel at very low levels. HP FeSi is therefore very well suited for the alloying of steels for ball bearings, plastic moulds, flapper valves, tire cord and grain oriented electrical steels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.60 g/cc0.0578 lb/in³
Density 3.20 g/cc0.116 lb/in³
Solubility in Water 0.00 %0.00 %Insoluble
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1100 J/g473 BTU/lb
Specific Heat Capacity 0.812 J/g-°C0.194 BTU/lb-°F
Melting Point 1205 - 1350 °C2201 - 2460 °F
Solidus 1205 °C2201 °F
Liquidus 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.050 %<= 0.050 %
Carbon, C <= 0.020 %<= 0.020 %
Iron, Fe >= 22.86 %>= 22.86 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si 75 - 77 %75 - 77 %
Sulfur, S <= 0.0030 %<= 0.0030 %
Titanium, Ti <= 0.050 %<= 0.050 %
 
Descriptive Properties
Angle of Repose40°-60°
Solubility in alkalisOxidizes with formation of H2 in Alkalis
Solubility in Hydrofluoric AcidSoluble with formation of SiF4
Solubility in Mineral AcidsSoluble with formation of H2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem HP FeSi 75 0.025 Ti High Purity Ferrosilicon
Elkem FeSi 0.50 Al Low Al Ferrosilicon
Titanium Ti-11.5Mo-6Zr-4.5Sn, ST 720°C, Aged 495°C
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 400°C
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 490°C

NELKEM23 / 16181

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.