Eastman Cadence™ GS4 is a high-flow amorphous copolyester for film calendering. Calendered films made of Eastman Cadence™ copolyester are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, coldforming, punching/cutting and embossment. Eastman Cadence™ resins require no pre-drying or additional stabilizers. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. Application/Uses - Appliance films
- Architectural laminates
- Automotive films
- Bags
- Decorative laminates
- Electronic laminates
- Floor coverings
- Furniture/Furniture trim
- Labels
- Outdoor films
- Packaging
- Printable films
- Shrink film
- Transaction cards
- Transportation laminates
- Wall coverings
Reported typical properties are preliminary. Information was provided by Eastman. |