Product Description: Fluon® TL-171E is a white PTFE (polytetrafluoroethylene) micropowder which is easy to disperse in a wide range of liquids. The reduced total surface areas of Fluon® TL-171E minimizes viscosity increase during mixing. The particles are soft, however, and retain good film forming capability. This combination of properties makes Fluon® TL-171E very useful in coating formulations. Fluon® TL-171E is suitable for use in food contact applications.Information provided by AGC Chemicals Americas Inc. |