MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 4202-15 MFR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: EMERGE™ PC 4202-15 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. It is available in 8 and 15 Melt Flow Rates. EMERGE™ PC 4202 resin is typically used in injection molding applications. Applications are information technology equipment, electrical parts, other structural/internal parts.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D792
Linear Mold Shrinkage 0.0020 cm/cmFlow; ASTM D955
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D785
Tensile Strength, Yield 12000 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 750000 psiASTM D638
Flexural Strength 21500 psiASTM D790
Flexural Modulus 720000 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 299 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 280 °Funannealed; ASTM D648
 288 °Fannealed; ASTM D648
Vicat Softening Point 318 °F50°C/hr, 50N; ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-0
@Thickness 3.05 mm
Oxygen Index 30 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 288 °C
Mold Temperature 82.0 °C
Drying Temperature 121 °C
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient LubriOne™ PC-20CF/15T Polycarbonate (PC)
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, 50% RH
Asahi Kasei Leona™ 13G25 Polyamide 66, GF Reinforced
Overview of materials for Polypropylene Copolymer

PZZDOW1338 / 30556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.