MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Lightweight Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Insulating Aggregate/Perlite raw material base. Hydraulic bond. A 1200°C insulating material with density and thermal conductivity designed to meet Petrochem lightweight specifications. Can be installed by casting, gunning or trowelling. Conforms to ASTM Class P.

Applications:

  • Backup insulation in two component linings in petrochemical process units
  • Hot face lining in ductwork from waste heat recovery boilers and process unit
  • F.C.C.U. linings – regenerator
  • Hydrogen or reducing atmosphere linings
  • Radiant section in steam flood generators
  • Steam flood generator convection sections and target walls
  • Cat cracker regenerator linings
  • Petrochemical applications

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.20 g/ccdried to 110°C
Grain Size <= 5000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 2.50 MPa
@Treatment Temp. 1400 °C
Cold Crushing Strength
 3.00 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
 3.50 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 5.00 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.370 W/m-K
@Temperature 600 °C
Maximum Service Temperature, Air <= 1200 °C
Shrinkage 0.00 - 0.20 %
@Treatment Temp. 110 °C
 0.30 %
@Treatment Temp. 815 °C
 0.70 %
@Treatment Temp. 1000 °C
 1.4 %
@Treatment Temp. 1400 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 32 %
CaO 12.1 %
Fe2O3 7.0 %
K2O+Na2O 2.3 %Na2O + K2O
MgO 0.60 %
SiO2 45 %
TiO2 1.8 %
 
Descriptive Properties
Net Material Required (kg/m³)1160
Water Addition35-38% by weight, 8.75-9.5L per bag, 25kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6377 / 203161

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.