MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Daikin DAI-EL® LT-252 Fluoroelastomer, 67% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes:

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/cc
Mooney Viscosity  30
@Temperature 121 °C
30
@Temperature 250 °F
ML1+10
 40
@Temperature 100 °C
40
@Temperature 212 °F
ML1+10
 42
@Temperature 100 °C
42
@Temperature 212 °F
Compound, ML1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6363peak
 58
@Time 3.00 sec
58
@Time 0.000833 hour
 60
@Treatment Temp. 250 °C,
Time 252000 sec
60
@Treatment Temp. 482 °F,
Time 70.0 hour
Air aging test
 62
@Treatment Temp. 230 °C,
Time 252000 sec
62
@Treatment Temp. 446 °F,
Time 70.0 hour
Air aging test
Tensile Strength at Break 13.5 MPa1960 psi
 5.13 MPa
@Treatment Temp. 250 °C,
Time 252000 sec
744 psi
@Treatment Temp. 482 °F,
Time 70.0 hour
Air aging test
 10.9 MPa
@Treatment Temp. 230 °C,
Time 252000 sec
1580 psi
@Treatment Temp. 446 °F,
Time 70.0 hour
Air aging test
Elongation at Break 280 %280 %
 305 %
@Treatment Temp. 230 °C,
Time 252000 sec
305 %
@Treatment Temp. 446 °F,
Time 70.0 hour
Air aging test
 456 %
@Treatment Temp. 250 °C,
Time 252000 sec
456 %
@Treatment Temp. 482 °F,
Time 70.0 hour
Air aging test
100% Modulus 1.80 MPa
@Strain 100 %
261 psi
@Strain 100 %
Tear Strength 43.0 kN/m245 pliangle type
Compression Set  8.0 %
@Temperature 25.0 °C,
Time 252000 sec
8.0 %
@Temperature 77.0 °F,
Time 70.0 hour
P-24 O-ring
 8.0 %
@Temperature 50.0 °C,
Time 252000 sec
8.0 %
@Temperature 122 °F,
Time 70.0 hour
P-24 O-ring
 10 %
@Temperature 100 °C,
Time 252000 sec
10 %
@Temperature 212 °F,
Time 70.0 hour
P-24 O-ring
 13 %
@Temperature 150 °C,
Time 252000 sec
13 %
@Temperature 302 °F,
Time 70.0 hour
P-24 O-ring
 17 %
@Temperature 175 °C,
Time 252000 sec
17 %
@Temperature 347 °F,
Time 70.0 hour
P-24 O-ring
 28 %
@Temperature 200 °C,
Time 252000 sec
28 %
@Temperature 392 °F,
Time 70.0 hour
P-24 O-ring
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -27.0 °C-16.6 °FLow Temperature Retraction, TR10
 -26.0 °C-14.8 °FGehman Torsion T10
 -21.0 °C-5.80 °FGehman Torsion T2
 -21.0 °C-5.80 °FLow Temperature Retraction, TR70
Brittleness Temperature -30.0 °C-22.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  2.00 min
@Temperature 160 °C
0.0333 hour
@Temperature 320 °F
Curelastometer, T90
 3.50 min
@Temperature 160 °C
0.0583 hour
@Temperature 320 °F
MDR, T90
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 67 %67 %
 
Descriptive Properties
Test Formula1TAIC
 1Peroxide
 100Polymer
 20N990 Carbon Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIJ9964 / 210037

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.