Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy molding formula is desired. 811 natural as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1). Information from manufacturer data sheet. Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line. |
Flexible, easy molding formula |