MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
660 Stainless Steel (A286) cold drawn wire diameter of 2.84 mm, aged at 425°C (800°F)
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 600 Series Stainless Steel

Material Notes: Test specimens were cold drawn and aged for 16 hours at temperature given, wire diameter of 2.84 mm, reduced in area by 80% of original diameter.

Key Words: UNS S66286 (UNS K66286), AMS 5525, AMS 5731, AMS 5732, AMS 5734, AMS 5735, AMS 5736, AMS 5737, AMS 5804, AMS 5805, ASME SA638, ASTM A453, ASTM A638, SAE J467 (A286); DIN 1.4980
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1482 MPa
Tensile Strength, Yield 1351 MPa
@Strain 0.2 %
Elongation at Break 9.5 %gage length is 4 times diameter
Reduction of Area 40 %
Modulus of Elasticity 200 GPaTypical for stainless steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.9 µm/m-°C
@Temperature 21.0 - 100 °C
solution treated, 16.7 solution treated and aged.
 17.2 µm/m-°C
@Temperature 20.0 - 250 °C
 17.4 µm/m-°C
@Temperature 21.0 - 500 °C
 17.6 µm/m-°C
@Temperature 21.0 - 650 °C
solution treated
 17.7 µm/m-°C
@Temperature 21.0 - 750 °C
solution treated
 18.5 µm/m-°C
@Temperature 21.0 - 750 °C
solution treated and aged.
 19.4 µm/m-°C
@Temperature 21.0 - 900 °C
solution treated
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 12.6 W/m-K
@Temperature 21.0 °C
 15.1 W/m-K
@Temperature 150 °C
 20.2 W/m-K
@Temperature 425 °C
 23.79 W/m-K
@Temperature 600 °C
 24.7 W/m-K
@Temperature 650 °C
Melting Point 1370 - 1425 °C
Solidus 1370 °C
Liquidus 1425 °C
Maximum Service Temperature, Air 815 °CContinuous Service
 980 °CIntermittent
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.035 %
Boron, B 0.0010 - 0.010 %
Carbon, C <= 0.080 %
Chromium, Cr 13.5 - 16 %
Copper, Cu <= 0.25 %
Iron, Fe 56 %
Manganese, Mn <= 2.0 %
Nickel, Ni 24 - 27 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
Titanium, Ti 1.9 - 2.35 %
Vanadium, V 0.10 - 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 425°C (800°F)
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 705°C (1300°F)
660 Stainless Steel (A286) cold drawn wire diameter of 5.61 mm, aged at 760°C (1400°F)
660 Stainless Steel (A286) cold drawn wire diameter of 2.84 mm, aged at 540°C (1000°F)
660 Stainless Steel (A286) cold drawn wire diameter of 2.84 mm, aged at 480°C (900°F)

MQ660BD / 13273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.