MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Melos Mecoline S TP 1028 F Halogen-free, thermoplastic, flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, flame retardant sheathing compound for low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: ATH

Standards: DIN EN 50363-8 TM7; VDE 0207 part 24 HM2; BS 7655 part 6.1 LTS 1 & LTS 3; IEC 60092-360 SHF 1; VDE 0250 part 215 HM 5

Typical applications: Halogen-free, low smoke, thermoplastic, flame retardant compound for the sheathing of low and medium voltage cables in General Installation applications. The compound features a high line speed and good processability.

Features: Flame retardant; Halogen-free; Low smoke

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³pressed plaques, 155°C / 5 min; DIN EN ISO 1183-1A
pH >= 4.5>= 4.5Corrosivity; IEC 60754-2
Mooney Viscosity 28
@Temperature 140 °C
28
@Temperature 284 °F
ML (1+4); DIN ISO 289-1
Melt Flow  11.5 g/10 min
@Load 21.6 kg,
Temperature 150 °C
11.5 g/10 min
@Load 47.6 lb,
Temperature 302 °F
DIN EN ISO 1133
 33.7 g/10 min
@Load 21.6 kg,
Temperature 190 °C
33.7 g/10 min
@Load 47.6 lb,
Temperature 374 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4747pressed plaques, 155°C / 5 min; DIN ISO 7619-1
Tensile Strength 10.9 MPa1580 psiextruded tapes; IEC 60811-501
 9.13 MPa
@Temperature 70.0 °C,
Time 605000 sec
1320 psi
@Temperature 158 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 11.597 MPa
@Temperature 100 °C,
Time 605000 sec
1682.0 psi
@Temperature 212 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-401
Elongation at Break 193 %193 %extruded tapes; IEC 60811-501
 158.07 %
@Temperature 100 °C,
Time 605000 sec
158.07 %
@Temperature 212 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 187.6 %
@Temperature 70.0 °C,
Time 605000 sec
187.6 %
@Temperature 158 °F,
Time 168 hour
extruded tapes, After ageing in air oven; IEC 60811-401
Penetration 6.0
@Temperature 80.0 °C,
Time 21600 sec
6.0
@Temperature 176 °F,
Time 6.00 hour
[%] Hot pressure test, extruded tapes; IEC 60811-508
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -25.0 °C-13.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 180 °C320 - 356 °FTool
 165 - 175 °C329 - 347 °FMaximum mass temperature
Zone 1 110 - 130 °C230 - 266 °F
Zone 2 120 - 140 °C248 - 284 °F
Zone 3 130 - 150 °C266 - 302 °F
Zone 4 140 - 160 °C284 - 320 °F
Zone 5 150 - 170 °C302 - 338 °F
Adapter Temperature 155 - 175 °C311 - 347 °F
Head Temperature 160 - 180 °C320 - 356 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 36 %36 %pressed plaques; ASTM D 2863 A
 
Descriptive Properties
Conductivity=10 µS/mmpressed plaques, 155°C / 5 min, IEC 60754-2
Main burning properties0Halogen content, IEC 754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS009 / 296116

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.