Hostacom BB 73 F C12360 is a 22% talc filled PP copolymer, with excellent flowability, high rigidity, high dimensional stability and good scratch resistance. Product is available as a customized color matched, pellet form. Applications: Interior Automotive Applications, Interior Trims.Information provided by LyondellBasell. |