Description: EVATHENE® UE659 is an ethylene-vinyl acetate copolymer resin (EVA) for use in injection, blown molding, and co-extrusion machine. Characteristics: - Flexibility
- Elasticity
- Great resistance to environmental stress cracking
- Low temperature flexibility
- Easy processability
Main Application: - Shoe sole foaming
- Hot melt adhesives
- Wire and cable compounds
Information provided by USI Corporation |