MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® K290ESD Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Tape; Thermoset; Polyimide, TS; Silicone

Material Notes: CHR® K290ESD is manufactured from polyimide film with high-temperature silicone adhesive.

Features/Benefits: CHR® K290ESD has excellent electrostatic discharge properties—the ESD additive reducing the electrostatic discharge that occurs upon tape removal. CHR® K290ESD can safely and cleanly be removed from printed circuit boards. The proprietary adhesive system provides high electrostatic dissipation without sacrificing adhesive strength at extreme temperatures. CHR® K290ESD offers excellent mechanical and electrical properties, an excellent dielectric strength and high conformability.

Applications: CHR® K290ESD is constructed to fill the requirements of a high performance Thermoplastic (Polyimide Backing Materials). CHR® K290ESD is chosen for gold finger protection during wave solder applications that require reduced electrostatic discharge upon tape removal.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 50 %
Tear Strength 30.0 pliInitial Tear Strength
Peel Strength 0.220 kN/mAdhesion to Steel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
Saint-Gobain CHR® K100 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape

PSTGQZ337 / 68851

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.