MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow SE SLR-4610 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SE SLR-4610 is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and non-staining stabilized. SE SLR-4610 is widely used in the tire industry for the manufacture of high performance tires providing excellent balance between rolling resistance and wet grip, but it is also used to manufacture high-quality technical rubber articles. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film. At mixing temperatures above 110°C, the rubber can be processed with the packaging film.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 2.5
@Temperature 160 °C
[dNm]; ML, (0.5 RAD); ASTM D5289
 4.5
@Temperature 160 °C
[min]; ts1, (0.5 RAD); ASTM D5289
 9.0
@Temperature 160 °C
[min]; T50, (0.5 RAD); ASTM D5289
 14.5
@Temperature 160 °C
[dNm]; MH, (0.5 RAD); ASTM D5289
 16
@Temperature 160 °C
[min]; T90, (0.5 RAD); ASTM D5289
Mooney Viscosity 45
@Temperature 100 °C
[MU]; ML 1+4, unmassed sample; ASTM D1646
Vinyl Acetate Content 63 %FTIR, internal method
Collected Volatile Condensable Material 0.35 %ASTM D5668
Storage Temperature <= 30.0 °C
 
Chemical PropertiesOriginal ValueComments
Styrene Content 25 %FTIR, internal method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 59
@Thickness 12.5 mm
(25 min / 160°C); ASTM D2240
Tensile Strength, Ultimate 19.0 MPaDie C (35 min / 145°C); ASTM D412
Tensile Stress at Strain 9.00 MPa
@Strain 300 %
ASTM D412
Elongation at Break 550 %ASTM D412
Rebound 15 %
@Thickness 12.5 mm
Schob pendulum, (25 min / 160°C); ISO 4662
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 198 °F
Glass Transition Temp, Tg -13.4 °FHR 10 K/min; half height; DSC
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
 
Descriptive Properties
Accelerator (TBBS) wt%1.38ASTM 3185-2B
Carbon Black wt%68.75ASTM 3185-2B; IRB 7
Stearic Acid wt%1ASTM 3185-2B
Sulfur content, %1.75ASTM 3185-2B
Total Extractables %27.2ASTM D5774
Zinc Oxide wt%3ASTM 3185-2B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SE SLR-4601 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Dow SE SLR-4400 Solution polymerized Styrene Butadiene Rubber (S-SBR)
Synthos SPRINTAN™ SLR 4630 Solution Styrene Butadiene Rubber (S-SBR)
Dow SE SLR-4610 H Solution polymerized Styrene Butadiene Rubber (S-SBR)
ATG s.r.l. SBR Styrene-Butadiene Rubber

PDOW1103 / 30307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.