MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical BPA
Categories: Fluid

Material Notes: Structure & Characteristics: (CH3)2C(C6H4OH)2 . BPA is an impetus powder with white color

Overview: Bisphenol-A(BPA) is used primarily to make polycarbonate and epoxy resins, both of which are used in a wide variety of application. Common examples of polycarbonate products include electronic and electrical component vehicles, CD/DVD and food and drink containers. In addition, epoxy resins are most commonly used as protective coatings, and adhesives. BPA is produced through a catalyzed condensation reaction of phenol with acetone.

CAS: 287-92-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
Bulk Density 0.630 - 0.680 g/cc
Molecular Weight 228.3 g/mol
Vapor Pressure 0.200 torr
@Temperature 170 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.10e+15 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 125 J/g
Specific Heat Capacity 1.51 J/g-°C
@Temperature 60.0 °C
 1.88 J/g-°C
@Temperature 157 °C
solid
 2.34 J/g-°C
@Temperature 165 °C
 2.55 J/g-°C
@Temperature 157 °C
liquid
Melting Point >= 156.5 °CFreezing Point
 157 °C
Boiling Point 360.5 °C
Flash Point 207 °CCOC
 227 °CCC
Ignition Temperature 532 °C
 
Descriptive Properties
Color<10 APHASolution color
 <20 APHAMolten color
 White prills
Explosion limit0.019 g/l
Purity>99.85T

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
Arlon Electronic Materials 45NK Woven Kevlar® Reinforced Laminate and Prepreg
Solvay CYCOM® 950-1 Epoxy Prepreg with 52% 285 Kevlar Fabric
Aluminum Chloride, AlCl3
Total Lacqtene® 2001 TBK 46 HDPE pipe

PLAY782 / 148792

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.