Description: Sealant tape. Ideally suited to aerospace and automotive applications. Features & Benefits: - Ideal oven and autoclave curing temperatures of up to 218°C (425°F)
- Good level of tack against all tool surfaces
- Excellent adhesion and “snap back” characteristics against all commonly used bagging films
- Strips very cleanly and quickly from mold surfaces, both hot and cold
- Manufactured by Schnee Morehead in the USA.