MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® 1495K with CAT 11 Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 1495K provides the following product characteristics:
  • Good thermal conductivity
  • Low viscosity
  • Can be used with a variety of catalysts

Application: Encapsulation, Potting

Loctite Stycast 1495K epoxy encapsulant formulated for use in applications requiring good flow performance and thermal conductivity. It is an excellent choice for transformers, sensors and other electronic assemblies that require good heat dissipation and protection from environment.

Loctite Stycast 1495K can be used with a variety of catalysts.

CATALYST DESCRIPTION

Loctite CAT 11 provides the following product characteristics:

  • Long pot life
  • Excellent chemical resistance
  • Good physical and chemical properties at elevated temperatures

Cure: Heat cure

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.89 g/ccMixed
 1.90 g/ccPart A, Loctite Stycast 1495K
Moisture Absorption 0.0900 %
@Time 86400 sec
Cured
Viscosity 47.5 cP
@Temperature 65.0 °C
Part B, Loctite CAT 11
Brookfield Viscosity 14000 cPMixed
 45000 cPPart A, Loctite Stycast 1495K; Spindle 6, speed 10 rpm
Linear Mold Shrinkage 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 95
Tensile Strength 59.0 MPa
Flexural Strength 87.0 MPa
Compressive Strength 190 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.60e+11 ohm-cm
@Temperature 130 °C
 5.00e+13 ohm-cm
@Temperature 25.0 °C
Dielectric Constant 4.09
@Frequency 1e+6 Hz
Dielectric Strength 15.7 kV/mm
Dissipation Factor 0.038
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µm/m-°C
Thermal Conductivity 1.25 W/m-K
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 1.00 hour
@Temperature 120 °C
Option 3
 2.00 - 4.00 hour
@Temperature 100 °C
Option 2
 8.00 - 16.0 hour
@Temperature 80.0 °C
Option 1
Working Life 240 min
@Temperature 25.0 °C
100 g
Shelf Life 12.0 MonthPart A, Loctite Stycast 1495K
 
Descriptive Properties
AppearanceBlack LiquidPart A, Loctite Stycast 1495K
Mix Ratio, by Volume100 : 9Material : Catalyst
Mix Ratio, by Weight100 : 5Material : Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7912 / 255399

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.