Daplen™ EG274AEB is a 24% mineral filled elastomer modified polypropylene compound intended for injection molding. Applications: Daplen EG274AEB has been developed especially for the car industry to be used in automotive exterior parts. - Automotive exterior applications
- Exterior trims
- Wheel arch and side trims
Special Features: - stiffness and impact balance
- UV resistance
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 95° - 105°C.Information provided by Borealis AG |