MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC SABIC® PC PC0703R PC (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. It is available exclusively at www.sabicpc.com

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.35 %23°C/sat; ISO 62
Moisture Absorption at Equilibrium 0.35 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039-2
 120ASTM D785
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 70 %50mm/min; ASTM D638
 >= 70 %50mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2350 MPa50 mm/min; ASTM D638
 2350 MPa1mm/min; ISO 527
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 90.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 900 J/mASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 70.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Dart Drop, Total Energy 65.0 Jpeak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 >= 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
IEC 60250
 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 27.0 kV/mm
@Thickness 1.60 mm
ASTM D149
 27.0 kV/mm
@Thickness 1.60 mm
IEC 60243-1
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 0.0010
@Frequency 60 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 70.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Thermal Conductivity 0.200 W/m-KASTM C177
 0.200 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 138 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
ASTM D648
Vicat Softening Point 144 °CRate B/50; ASTM D1525
 144 °CRate B/50; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
 1.586ASTM D542
Haze <= 0.80 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 - 90 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 280 - 310 °CInjection Molding
Zone 1 260 - 280 °CProfile Extrusion
 270 - 300 °C
Zone 2 260 - 280 °CProfile Extrusion
 280 - 310 °C
Zone 3 260 - 280 °CProfile Extrusion
 290 - 320 °C
Zone 4 260 - 280 °CProfile Extrusion
Adapter Temperature 260 - 280 °CProfile Extrusion
Die Temperature 250 - 260 °CProfile Extrusion
Melt Temperature 270 - 280 °C
 290 - 320 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 120 °CProfile Extrusion
 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 2.00 - 4.00 hourProfile Extrusion
Moisture Content 0.020 %
 0.020 %
Precipitation Temperature 70.0 - 90.0 °CCalibrator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10705 / 244172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.