MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-FLEX 602 Conductive Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: CHO-FLEX™ 602 is a two-component silver-filled polyurethane coating designed for room temperature or oven cure. CHOFLEX™ 602 coating can be sprayed on large panels, cured at room temperature and coated with most military grade urethane or epoxy top coats. It can also be sprayed on most thermoplastic enclosures such as PPO, ABS, polystyrene and polycarbonate.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 g/cc
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.060 ohm
Shielding Effectiveness 60 - 70 dB
@Frequency 1.00e+8 - 1.00e+9 Hz
on epoxy/glass or epoxy/graphite
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 107 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 25.0 °C
Shelf Life 6.00 Month
 
Descriptive Properties
BinderPolyurethane
ConsistencyThixotropic Paste
FillerAg
Mix Ratio100:13
Theoretical Coverage4320 in2 / lbActual coverage will be 50-100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 50 pcf
Covestro Baydur® 426 IMR RIM system
Coastal Enterprises Plus™ PBLT-75 High Density Urethane Foam
C.O.I.M. UREXTER® Lp 2500_30 Polyurethane Two-Component Compound
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting

PCHOME072 / 28294

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.