MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)  (discontinued **)
Categories: Polymer; Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resistant and blended for toughness. The raw materials used in the manufacture of this resin are listed as acceptable in FDA regulatory Title 21 CFR 177.2420 for repeated use in contact with food subject to compliance with the prescribed limitation of that regulation.

Performance:
  • Excellent corrosion resistance
  • Excellent impact strength
  • High tensile elongation
  • FDA application


Properties listed typical cured casting, catalyzed with 1% BPO, cured two hours at 160°F then one hour at 200°F, post cured two hours at 280°F. See also: "Vinyl Ester Resin (Laminate Properties)" for information on that application.

Can be used for hand lay-up and spray-up, filament winding, flake glass and filled lining and coating compounds. Perfect for repairing tank linings, blistering boat hulls, and fabricating tough all-around parts.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccLiquid Property
Solids Content 52 %Liquid Property
Viscosity 275 cPLiquid Property
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 35ASTM D2538
Tensile Strength at Break 120000 psiASTM D638
Elongation at Break 7.9 %ASTM D638
Elongation at Yield 4.6 %ASTM D638
Tensile Modulus 540000 psiASTM D638
Flexural Strength 19000 psiASTM D790
Flexural Modulus 500000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 98.0 °CDeflection Temp; Load not specified; ASTM D648
Flash Point 73.0 - 100 °FLiquid Property
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6063-T6
BCC Products BC 8675E Polyurethane Elastomer
AISI 1045 Steel, Quenched and Tempered to 390 HB
BCC Products BC 8690E Polyurethane Elastomer
BCC Products BC 8860 Polyurethane Elastomer

PFIBRE44 / 38303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.