Data provided by the manufacturer, Exxon Chemical. A crosslinkable polyethylene homopolymer designed as an electrical grade base resin especially suitable for Henschel blending. Applications: A base resin for fully formulated crosslinkable medium voltage cable insulation compounds. |
Low Density Polyethylene; Exxon Chemical Company |