MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Methyl acrylate, C4H6O2
Categories: Fluid; Solvent

Key Words: C4H6O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc
@Temperature 20.0 °C
0.0345 lb/in³
@Temperature 68.0 °F
Viscosity 0.501 cP
@Temperature 20.0 °C
0.501 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 86.091 g/mol86.091 g/mol
Vapor Pressure 0.088238 bar
@Temperature 20.0 °C
66.184 torr
@Temperature 68.0 °F
Surface Tension 24.2 dynes/cm
@Temperature 20.0 °C
24.2 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 42.6 bar31900 torr
Critical Temperature 263 °C505 °F
Critical Density 0.325 g/cc0.0117 lb/in³
Critical Molar Volume 265 cm³/mol16.2 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 371.8 J/g159.9 BTU/lb
Specific Heat Capacity 1.048 J/g-°C
@Temperature 25.0 °C
0.2505 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1586 W/m-K
@Temperature 20.0 °C
1.101 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -76.5 °C-106 °F
Boiling Point 80.4 °C177 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.403
@Wavelength 589.3 nm
1.403
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.1088
Antoine's Vapor Pressure B Parameter2788.43
Antoine's Vapor Pressure C Parameter-59.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)96-33-3
Chemical FormulaC4H6O2
Critical Compressibility (Zc)0.25
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A451.02
Dynamic Viscosity Parameter B245.3
Henry's Law Constant (atm m3/mol)0.000188
Molar Heat Capacity (298K)90.198 J/mol-K
Molar Heat Capacity of Vapor a Parameter15.1544
Molar Heat Capacity of Vapor b Parameter0.2794
Molar Heat Capacity of Vapor c Parameter-8.799E-05
Molar Heat Capacity of Vapor d Parameter-1.659E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1919

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VORGS219 / 99585

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.