NAV101M is a transparent low density post-consumer recycled (rLDPE) supplied in pellet form for high-end blown film applications. NAV101M is an ideal LDPE used where sustainability and circularity matter. NAV101M is 100 % post-consumer recycled including a majority of pre-sorted municipal (household) waste. NAV101M is part of the EuCertPlast certificate according to the European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color and other product properties can be observed between batches. Cas No. 9002-88-4 Typical characteristics: - High transparency
- Pellet shape: lenticular
- Low odor
- Filtration 100 µm
- Available in homogenized 24-ton truckloads
Applications:- Collation shrink film
- Shrink film
- Lamination films for non food contact primary packaging
- Non food contact primary packaging
- Secondary and tertiary packaging where transparency is key parameter
Note: Minor quantity of BorShape" LLDPE significantly boosts mechanical performances of NAV101 helping convertors, brand owners and retailers meeting their sustainability goals without compromising key mechanical properties for similar packaging performance.Information provided by Borealis AG |